MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
TIMET TIMETAL® 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4987
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: High-Strength Forging Alloy. Mechanical property data reported per ASTM 4987 after solution treatment and aging 1050°-1100°F (566°-593°C) then air cool.

Industry Specifications: USA Aerospace: AMS 4987.

Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and high cycle fatigue strength. Typically used for critical aircraft structures, such as landing gear, actuators, flap tracks, and rotor heads.

Typical heat treatment for this alloy: Solution heat treat: 28-56°C below beta transus for a minimum for 30 mins, then water quench. Age then air cool.

Data provided by TIMET.

Vendors:
Available Properties
  • Density, Typical
  • Tensile Strength, Ultimate, Typical
  • Tensile Strength, Yield, Typical
  • Elongation at Break, Typical
  • Reduction of Area
  • Tensile Modulus
  • Tensile Modulus
  • Compressive Yield Strength
  • Compressive Modulus
  • Ultimate Bearing Strength, e/D = 1.5
  • Ultimate Bearing Strength, e/D = 2.0
  • Bearing Yield Strength, e/D = 1.5
  • Bearing Yield Strength, e/D = 2.0
  • Poissons Ratio
  • Fatigue Strength, Limit; test specifics not reported
  • Fracture Toughness, ST then Aged 8 hrs
  • Shear Modulus
  • Shear Strength
  • CTE, linear
  • Beta Transus
  • Aluminum, Al
  • Carbon, C
  • Hydrogen, H
  • Iron, Fe
  • Nitrogen, N
  • Other, total
  • Other, total
  • Oxygen, O
  • Titanium, Ti, Calculated as remainder
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.