Colorless polyimide with high temperature stability. NeXolve Novastrat® 400 is a colorless polyimide with a higher temperature stability than NeXolve’s LaRC™CP1, exhibiting a glass transition temperature exceeding 350°C. These properties lend Novastrat® 400 for a wide variety of uses in display applications, space structures, thermal insulation, electrical insulators, industrial tapes and advanced composites. For applications requiring transparency, traditional polyimides are highly absorptive in the UV and blue region, and absorb significant amounts of energy, leading to high thermal loads. Novastrat® 400, however, is much less absorptive and provides much less lower thermal loads and higher optical transparency. Additionally, Novastrat® 400 is solvent soluble and can be spray-applied and cured at low temperatures while retaining high temperature stability typical of polyimide films. Novastrat® 400 is provided as a film or liquid resin for spray or flow casting operations. Information Provided by NeXolve Corporation. |