MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
LyondellBasell Petrothene® YR19548 Polyolefin Compound
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes:

Applications
PETROTHENE YR 19548 is a colorable, thermoplastic non-halogenated, flame retardant polyolefin compound formulated for small gauge automotive primary insulation (SAE J1128) and appliance wire insulation when crosslinked by radiation. YR 19548 permits high line speeds (3.000 fpm) and extremely fast cure speeds (6,000 fpm).

Processing Techniques
YR 19548, like other thermoplastic polyolefin compounds, can be extruded as wire and cable jacketing using a conventional extruder. Crosslinking may be achieved by using electron beam radiation. Below are suggested extrusion and curing conditions for YR 19548. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size, radiation unit design and cable constructions all have an effect on processing of crosslinkable compounds.

Additional Suggestions
Maximum screen pack of 40 mesh
Little or no die land
No predrying normally required
Compression ratio 2:1-3:1
"Mixing" screw can be used if properly designed to prevent excessive heat build-up
Suggested radiation dosage: 7.5 MRads

Physical Properties
All properties determined form #20 AWG/TXL wire irradiated at 7.5 MRads. The data obtained for physical and electrical properties are nominal values only and are subject to normal variations consistent with the test methods and/or variations found acceptable to the industry.

This product is from the former Equistar product line.

Key Words: Automotive SAE J1128; Irradiated Cure
Vendors:
Available Properties
  • Density, ASTM D1505
  • Tensile Strength at Break, ASTM D638, 100% retained after aging 7 days at 165°C.
  • Elongation at Break, ASTM D638, 90% of original retained after aging 7 days at 150°C.
  • Feed Temperature
  • Zone 2
  • Zone 3
  • Zone 4-x
  • Adapter Temperature
  • Die Temperature
  • Melt Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.