MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
DowAksa CarbonBond™ 200P Adhesive Putty System
Categories: Polymer; Thermoset; Epoxy

Material Notes: CarbonBond™ 200P is a high strength, toughened, structural epoxy adhesive for bonding of composite fabrics to substrate. CarbonBond™ 200P is a two phase (toughened) epoxy resin produced using a CTBN elastomer and a flexible resin backbone for maximum stress and fatigue resistance. CarbonBond™ 200P bonds with an immediate high tack consistency, a long working life and a quick cure time. The hardener provides >2 hour working life with full cures occurring between 6 hours to 7 days, depending on the cure temperature. It is recommended that the minimum application temperature should be at least 3°C above the dew point temperature. Unlike most epoxy adhesives, CarbonBond™ 200P adhesive cured at ambient temperatures provides heat resistance well in excess of most engineering limits (HDT of 180º F).

Information provided by DowAksa.

Vendors:
Available Properties
  • Density, Part B
  • Density, Part A
  • pH, Part A
  • pH, Part B
  • Hardness, Shore D
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Adhesive Bond Strength, to concrete
  • Maximum Service Temperature, Air, HDT load not reported
  • Glass Transition Temp, Tg, ASTM E1640
  • Cure Time, Initial
  • Pot Life, 1000g working life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.