Uses: Profiles and Sheet
Processing Method: Extrusion, Profile and Sheet
Information provided by M. Holland.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic