MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman EP Solvent, Stabilized
Categories: Fluid; Solvent

Material Notes: CAS No. 2807-30-9

Product Description: Eastman™ EP Solvent (Ethylene Glycol Monopropyl Ether) is a colorless, water-miscible solvent providing a slow evaporation rate, good viscosity control in waterborne resins, and high flash point. Eastman™ EP Solvent has a milder, less detectable odor than most other glycol ethers, enhancing its use in coatings when mild odor is desirable. Eastman™ EP Solvent is completely water miscible over a wide range of temperatures. Eastman™ provides this solvent stabilized with

  • BHT (butylated hydroxytoluene).

    Application/Uses:

    • Aerosols
    • Cleaners - Ink Processes, Glass, Household, Industrial, and Metal
    • Coatings - Automotive OEM
    • Coatings - Automotive Refinish
    • Coatings - Can and Coil
    • Coatings - Consumer Electronics
    • Coatings - General Industrial
    • Coatings - Industrial Maintenance and Marine
    • Coatings - Industrial Wood
    • Coatings - Transportation
    • Graphic Arts - Printing Inks
    Key Attributes:
    • Good coupling efficiency
    • Good solvent activity
    • High dilution ratio
    • Inert - Nonfood use
    • Low surface tension
    • Low volatility/Low vapor pressure
    • Miscible with water and most organic liquids
    • Predicted to be biodegradable*
    • REACH compliant
    • Slow evaporation rate

    Information provided by Eastman

  • Vendors:
    Available Properties
    • Density
    • Molecular Weight
    • Total Acid Number
    • Melting Point, Freezing Point
    • Boiling Point, @ 760 mm Hg, Initial
    • Boiling Point, @ 760 mm Hg, Dry Point
    • Flash Point, Tag Closed Cup
    • Flash Point, Tag Open Cup
    • Refractive Index
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Proto3000 – 3D Engineering Solutions
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.