Notes: Medalist MD-16150G XRD1 is a high performance thermoplastic elastomer specifically designed for healthcare and medical applications. Medalist MD-16150G XRD1 is a low hardness, low density, tack-free grade that can be sterilized and is suitable for injection molding. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Chemical Resistant; Ethylene Oxide Sterilizable; Good Colorabiilty; Good Moldability; Good Processability; Good Toughness; Halogen Free; High Elongation; High Flexibility; High Flow; Low Density; Low Hardness; Resilient; Soft; Tack Free Uses: Disposable Hospital Goods; Medical Devices; Rubber Replacement; Soft Touch Applications; Surgical Instruments Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |