MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, Annealed at 982°C (1800°F), UNS N06601
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increased chromium, an aluminum content which together provide outstanding resistance to oxidation. In addition, AL 601 alloy has good resistant to environments containing carbon and sulfur and this alloy resists aqueous corrosion. The AL 601 alloy is used in aerospace applications, for heat and chemical processing equipment, and in power generation, pollution control and heat treating applications. Forming, machining and welding properties are similar to those of stable austenitic stainless steels.

Information provided by Allegheny Ludlum

Key Words: DIN 2.4851; ASTM B-168; AMS 5870
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, Typical
  • Tensile Strength, Ultimate, Typical
  • Tensile Strength, Yield, Typical
  • Elongation at Break, typical in 2"
  • Reduction of Area, Typical
  • Modulus of Elasticity
  • Charpy Impact, Typical
  • Magnetic Permeability
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Maximum Service Temperature, Air, High oxidation resistance due to tenacious oxide film formation.
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ATI Allegheny Ludlum, Allegheny Technologies Incorporated

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.