MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Tra-Con Tra-Bond 1137 Epoxy Microballoon Repair Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 1137 is a sag resistant syntactic-foam formulation developed for aerospace honeycomb, fillet, edge-fill, contour repair, bonding, potting and casting applications where a light-weight, low shrinkage and low expansion material is required. This adhesive is easily mixed and handled at room temperature, and it develops strong, highly reliable bonds to most surfaces -- including metals, glass and glass fabrics, and many plastics. TRA-BOND 1137 is a completely unicellular material composed of micron-sized phenolic spheres in a high-performance epoxy binder, has a very uniform point-to-point structure and exhibits low shrinkage during cure, good dimensional stability, low density, high strength-to-weight ratio, high dielectric strength, and a low dielectric constant. The fully cured adhesive is a strong, light weight and durable electrical insulator which can be cut, drilled sawed and shaped (as needed) with ordinary shop tools. In addition, TRA-BOND 1137 is resistant to water, weather, gases and vapors, salt and salt solutions, mild acids and alkalis, alcohol, jet fuels, gasoline and other petroleum products, and many other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Hardness, Shore D
  • Cure Time
  • Cure Time
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.