MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Morgan Advanced Ceramics Cerablanketâ„¢ Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: All three grades of blanket have the same excellent chemical stability compared with their raw materials: Cerafiber, Cerachem Fiber and Cerachrome Fiber spun bulk. They have excellent strength before and after heating. They have superior acoustic as well as thermal insulation characteristics. The wide range of available densities and thicknesses allow for the most effective deployment of the superior thermal characteristics in a wide variety of applications.

Applications:

  • Furnace and kiln linings
  • Boiler insulations
  • Heat treatment temperature control
  • Glass furnace crown insulation
  • Furnace door seals
  • Duct linings
  • Pipe insulations
  • Thermal barriers for automotive industry
  • Insulation for field stress relieving of welds
  • High temperature filter media
  • Nuclear insulation applications
  • Steam and gas turbines insulation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density, EN 1094-1, 4 densities available
  • Tensile Strength, EN 1094-1, at 64 kg/m3
  • Tensile Strength, EN 1094-1, at 96 kg/m3
  • Tensile Strength, EN 1094-1, at 128 kg/m3
  • Tensile Strength, EN 1094-1, at 160 kg/m3
  • Specific Heat Capacity
  • Thermal Conductivity, at 96kg/m3
  • Thermal Conductivity, at 128kg/m3
  • Thermal Conductivity, at 64kg/m3
  • Thermal Conductivity, at 160kg/m3
  • Thermal Conductivity, at 128kg/m3
  • Thermal Conductivity, at 96kg/m3
  • Thermal Conductivity, at 64kg/m3
  • Thermal Conductivity, at 160kg/m3
  • Thermal Conductivity, at 128kg/m3
  • Thermal Conductivity, at 96kg/m3
  • Thermal Conductivity, at 160kg/m3
  • Thermal Conductivity, at 128kg/m3
  • Thermal Conductivity, at 64kg/m3
  • Thermal Conductivity, at 96kg/m3
  • Thermal Conductivity, at 160kg/m3
  • Thermal Conductivity, at 128kg/m3
  • Thermal Conductivity, at 64kg/m3
  • Thermal Conductivity, at 96kg/m3
  • Thermal Conductivity, at 64kg/m3
  • Shrinkage, isothermal
  • Shrinkage, isothermal
  • Shrinkage, isothermal
  • Shrinkage, isothermal
  • Al2O3
  • CaO+MgO
  • K2O+Na2O
  • Other, Fe2O3+TiO2
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.