MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Kohesi Bond KB 1085-1 Two component, graphite filled, electrically conductive epoxy for bonding and sealing
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Highlights:
  • Graphite filled, electrically conductive
  • Non-magnetic
  • Offers good lubricity
  • Ideal for static dissipation and grounding
  • First-rate dimensional stability
  • Very good shielding against EMI/RFI
Kohesi Bond KB 1085-1 is a two component, graphite filled epoxy system suitable for bonding, sealing and coating. It has a favorable 100:15 (Part A: Part B) mix ratio by weight. Firstly, it offers very good electrical conductivity and a outstanding dimensional stability. This epoxy system readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. KB 1085-1 offers a volume resistivity of 50 - 100 ohm-cm. This makes it ideal for static dissipation, grounding and EMI/RFI shielding applications. Being graphite filled, this product is non-magnetic in nature and offers slight lubricity. It offers an extensive service temperature range of -50°C to +120°C. It is an adhesive that offers superb physical strength properties and adheres well to a wide variety of substrates including metals, ceramics, most plastics and glass. In addition to superior electrical, it also offers excellent chemical resistance to a variety of acids, bases, oils and water. Part A and Part B are black in color. Owing to its versatile performance, KB 1085-1 is widely used in electronics, aerospace, semiconductor, microwave and many OEM applications where a non-metallic conductive epoxy is required.

Typical Applications:

  • Bonding
  • Sealing
  • Coating

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Volume Resistivity
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Option 2
  • Cure Time, Optimum Cure: overnight at 23°C plus 3 - 5 hours at 70°C - 90°C
  • Cure Time, Option 1
  • Working Life, 100 g of mixed epoxy
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.