Availability: North America
Filler/Reinforcement: Mineral, 26% Filler by Weight
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic