MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Raschig Group 5557 DAP  (discontinued **)
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled; Filled/Reinforced Thermoset

Material Notes: Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot humid conditions, long term retention of dimensional stability also under severe environmental conditions. Self-extinguishing (V-0/0,6 according to UL 94). Free of toxic heavy metals. Forms: Low dust granulate packed in moisture resistant cartons. Standard carton size: 20 kg palletized in 600 kg loads. Processing: Injection and transfer.

Applications:

  • Connectors
  • Bobbins
  • Potentiometers
  • Switches
  • Information provided by the Raschig Group

    Vendors:
    Available Properties
    • Specific Gravity, ISO 1183
    • Apparent Bulk Density, ISO 60
    • Linear Mold Shrinkage, ISO 2577, Injection
    • Flexural Strength, ISO 178, Injection
    • Flexural Modulus, ISO 178, Injection
    • Compressive Strength, ISO 604
    • Charpy Impact Unnotched, ISO 179/ 1eU, Injection
    • Surface Resistance, IEC 60093
    • Dielectric Constant, IEC 60250
    • Dielectric Strength, IEC 60243-1
    • Dissipation Factor, IEC 60250
    • Comparative Tracking Index, IEC 60112, CTI-M
    • Comparative Tracking Index, IEC 60112
    • CTE, linear, ISO 11359-2
    • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-A, Injection
    • Flammability, UL94
    • Shrinkage, ISO 2577, Post-shrinkage
    • Front Barrel Temperature
    • Melt Temperature
    • Mold Temperature
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.