Description: A-910p is an expandable polystyrene grade containing pentane as a blowing agent. It is a special, antistatic grade. The products are delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3 and is available in 1100 kg octabins. Applications: The properties of A-910p make it suitable for the production of thin-walled shape-moulded products especially for the electrical industry, where the antistatic behaviour of packaging material is needed. Information provided by BEWi Synbra |