MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Omnia Plastica Akulon® PA 66.6 - Akulon GX - at 50% RH
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tools and on CNC centres. The U.V. stabilisation makes it light resistant and it is therefore suitable for outdoor applications.

Features:

  • Wear resistance: good even in demanding environments. Toughness: high tensile stress and compressive strength.
  • Self-lubricating: the friction coefficient is low and generally for sliding application it does not require lubricators.
  • U.V. resistance: particularly suitable for outdoor applications it withstands atmospheric agents and low temperatures very well.
  • Machining on automatic tools is easy thanks to the breaking of shavings during machining and to its higher stiffness.
  • Black colour.
Weak Point:

It is hygroscopic (even if at lower extent than PA6) therefore the mechanical features and the dimensions will change consequently

Application:

  • Mechanical: thanks to its higher stiffness compared to PA6 and its higher shock resistance compared to PA66, this material is increasingly being used in the mechanical field to produce gears, cams, pulleys, anti-wear guides, wheels and other components, notably for outdoor use. In the field of construction and earthmoving equipment Akulon GX can be found in guides, bearings and pulleys. it is particularly suitable for machining on automatic lathes.
  • Food contact: generally it is not used in contact with food.
  • Electrical: use in the electrical field is to be avoided as the electrical features change with the moisture content. It is sometimes used when its mechanical features are required.
  • Chemical: it is resistant to alkali, inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors:
Available Properties
  • Density, ISO.1183 DIN.53479
  • Moisture Absorption at Equilibrium, 50% relative humidity (beginning dry)
  • Water Absorption at Saturation, 23°C (beginning dry)
  • Ball Indentation Hardness, ISO2039.1 DIN.53456
  • Tensile Strength at Break, ISO.527 DIN.53455
  • Elongation at Break, ISO.527 DIN.53455
  • Tensile Modulus, ISO.527 DIN.53455
  • Compressive Strength, ISO.899 DIN.53444, 1% strain over 1000 hours
  • Charpy Impact Unnotched, ISO.R179 DIN.53453, 7.5 J
  • Charpy Impact, Notched, ISO179/3C DIN.53453
  • Coefficient of Friction, Dynamic, on dry ground steel; load =0.05MPa; speed =0.6 m/s (dry sample)
  • Dielectric Constant, ISO.250 DIN.53483
  • CTE, linear, dry sample
  • Thermal Conductivity, DIN.52612 (dry sample)
  • Melting Point
  • Maximum Service Temperature, Air, Continuous; 5000 hours based on a tensile stress of 50% at 23° C. (dry sample)
  • Maximum Service Temperature, Air, short period, no load (dry sample)
  • Deflection Temperature at 1.8 MPa (264 psi), ISO.75 DIN.53461 (dry sample)
  • Minimum Service Temperature, Air, impact conditions and heavy loads not considered (dry sample)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Omnia Plastica s.p.a.

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.