Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additives Characteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blended with LDPE or HDPE Applications: thick or thin film applications where excellent toughness and abuse resistance, hot-tack and heat seal properties are required Natural Color Slip: 1000 ppm Antiblock: 3000 ppm. Recommended processing conditions: 6.35 cm extruder. 24:1 screw L/D ratio. 0.203 cm die opening. Melt temperature 232°C. Blow up ratio 2.5:1. Output rate 8.0 lb/hr/in die cir. Hot-Tack Initiation Temperature: 85°C Ultimate Hot-Tack Strength: 3.1 N Heat Seal Initiation Temperature at 0.5 lb.: 97°C Ultimate Heat Seal Strength: 9.5 N. Film properties based on thickness of 0.0318 mm. Information provided by Chevron Phillips Chemical Company. |