MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Evonik SITREN® MR 870 Emulsion
Categories: Other Engineering Material

Material Notes: Product description: SITREN® MR 870 is an emulsion concentrate based on biodegradable oils for the formulation of environmentally friendly mould release emulsions.

Applications:

  • Concentrate for the formulation of stable mould release emulsions.
  • Mould release agent for on-site use in precast industry.
Properties/Benefits: SITREN® MR 870 reduces the adhesion between concrete and mould resulting in minimum cleaning and wear of the mould yielding improved surface properties of the concrete at the same time. Additionally, SITREN® MR 870 provides the following benefits and advantages:
  • Readily biodegradable according to OECD criteria
  • Smooth surface
  • Reduced number of pin holes and other surface defects
  • No discoloration of the concrete surface
  • Reduced dust build-up on moulds - resulting in a cleaner surface and less cleaning cycles
  • For horizontal and vertical cast concrete applications
  • Easy to dilute and apply
  • Dilutions of SITREN® MR 870 exhibit excellent storage stability (tap water may be suitable)
  • Reduced health and environmental risks due to biodegradable oil

Information provided by Evonik

Vendors:
Available Properties
  • Density
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.