MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
ChevronTexaco Cetus® PAO 46
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Texaco Cetus PAO oils deliver value through:
  • Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.
  • Extended machinery life and increased compressor efficiency — Oxidative stability and low carbon-forming tendencies minimize sludge and deposit formation.
  • Extended drain intervals — Long lubricant life means less frequent oil changes.
  • Reduced maintenance and downtime — Trouble free operation and extended service intervals means reduced operating costs.
  • Reduced oil consumption — Low volatility means less oil goes downstream, and less oil is needed for makeup.
  • Recommended in Atlas Copco, Sullair, Ingersoll-Rand and Quincy rotary screw air compressors. Texaco Cetus PAO products meet the requirements of German DIN 51506 VDL standard.

    Texaco Cetus PAO oils are synthetic compressor oils. They are based on polyalphaolefin technology.

    They provide outstanding thermal and oxidation stability, high viscosity index, high flash point, low pour point, and excellent hydrolytic stability.

    Texaco Cetus PAO oils protect against rust, oxidation, and foaming, and have good antiwear properties.

    The natural thermal and oxidation stability of these lubricants, due to their high level of purity and refinement, has been further enhanced by their unique additive systems.

    The high thermal and oxidation stability reduces the formation of oxidation byproducts and acidic materials which will eventually cause deposits and varnish.

    They are able to withstand relatively high temperature operations for extended periods of time. They have very good demulsibility characteristics allowing quick release of moisture.

    They minimize entrained air, which could otherwise result in reduced lubricant film thickness and potentially lead to pump cavitation.

    They are compatible with most elastomeric seal materials that are used with mineral oil based compressor lubricants.

    Texaco Cetus PAO oils are formulated to provide outstanding lubricating qualities for air compressors, especially portable and stationary rotary, vane, and screw compressors.

    Texaco Cetus PAO oils are recommended for industrial bearings and gears that require a synthetic gear oil that does not contain extreme pressure additives.

    Texaco Cetus PAO oils are designed for applications with wide operating temperature ranges. They are especially effective in high temperature applications where outstanding thermal and oxidative stability are required.

    Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

    Do not use in breathing air apparatus or medical equipment.

    Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

    CPS Number: 222022; MSDS Number: 8903

Vendors:
Available Properties
  • API Gravity, ASTM D287
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Saybolt Viscosity at 100°F, ASTM D445
  • Saybolt Viscosity at 210°F, ASTM D445
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Oxidative Stability, ASTM D2272, to 25 psi drop
  • ASTM Color, ASTM D1500, L
  • Four Ball Wear, ASTM D4172, Scar Diameter, 1800 rpm, 20 kg
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.