MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: TU3002 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties (dart drop and Elmendorf tear strength), and good processability. These qualities ensure the production of films with uniform thickness. TU3002 resin is stabilized with a synergistic combination of a hindered amine (HALS) with UV absorbers and antioxidants which warrant high resistance to aging caused by exposure to solar radiation. Films manufactured with TU3002 are colorless and have high light transmission. This product is identified as PE 115 according to ASTM D-4976-04a standard specification. It contains antioxidant and anti-UV additives. Its applications include films for covering greenhouses and agricultural tunnels and films for applications that require high mechanical strength and high resistance to aging from solar radiation (UV radiation exposure). Films manufactured with TU3002 have a minimum duration expectancy of 18 months (two winters and one summer) for continuing use in a greenhouse with a maximum solar radiation of 150 kLy (kcal/cm²/year) and at least 130µm. The suitable durability refers to the retention of at least 50% of the original mechanical resistance of a film produced with pure TU3002. The UV stabilizer used in TU3002 presents great chemical resistance for a range of pesticides, although compounds which have sulfur and halogens can reduce the films' shelf life.

Vendors:
Available Properties
  • Density, ASTM-D792
  • Melt Flow, ASTM-D1238
  • Film Elongation at Break, MD, ASTM-D882
  • Film Elongation at Break, TD, ASTM-D882
  • Secant Modulus, MD, ASTM-D882, 2% Secant Modulus
  • Secant Modulus, TD, ASTM-D882, 2% Secant Modulus
  • Elmendorf Tear Strength MD, ASTM-D1922
  • Elmendorf Tear Strength TD, ASTM-D1922
  • Elmendorf Tear Strength, MD, ASTM-D1922
  • Elmendorf Tear Strength, TD, ASTM-D1922
  • Dart Drop, ASTM-D1709 (Method B)
  • Dart Drop Test, ASTM-D1709 (Method B)
  • Film Tensile Strength at Break, MD, ASTM-D882
  • Film Tensile Strength at Break, TD, ASTM-D882
  • Haze, ASTM-D1003
  • Gloss, ASTM-D2457, Angle 60°
  • Die Opening, Blow Film Extrusion
  • Blow-up Ratio (BUR), Blow Film Extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.