MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay CYCOM® 5250-4 BMI Prepreg System with IM7-6K-5HS Woven Carbon Fiber
Categories: Polymer; Thermoset; Bismaleimide (BMI); Carbon Fiber/Thermoset Composite

Material Notes: 58 Volume % IM7-6K-5HS.

CYCOM® 5250-4 is a 350°F to 400°F (177°C to 204°C) curing bismaleimide resin with a service temperature range of -75°F to 400°F (-59°C to 204°C). CYCOM 5250-4 is specifically formulated for use in primary aircraft structures. In addition, a variety of secondary structural components can take advantage of the increased performance from using high-strain carbon fibers and the improved damage-resistance this system provides. CYCOM 5250-4 is available with either carbon fiber or glass fiber reinforcement in unidirectional tape, woven broadgood and roving forms.

Features & Benefits:

  • Short-term service temperature up to 450°F (232°C)
  • Superior hot/wet properties at 220°F to 375°F (104°C to 190°C)
  • Excellent toughness
  • Void-free laminates
  • High temperature resistance
  • Low thermal conductivity
  • Versatile cure
  • Excellent compression strength properties after impact
  • Shop life greater than 28 days at room temperature
  • Fluid/solvent resistant
Suggested Applications: Primary and secondary aircraft structure including:
  • Engine nacelles
  • Fuselage skins and stiffeners
  • Wing and stabilizer spars and skins
  • Other critical load-bearing components
Mechanical properties are reported for standard cure + standard post-cure

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, QC-PT-55, Neat Resin
  • Volatiles
  • Water Absorption, As Tested (Wet)
  • Tensile Strength, Open Hole, (+,0,0,90,0), IM-7-6K-5HS, Wet
  • Tensile Strength, Open Hole, (+,0,0,90,0), IM-7-6K-5HS
  • Tensile Strength, Fill (90°), IM-7-6K-5HS, Wet
  • Tensile Strength, ASTM D3039, Warp (0°), IM-7-6K-5HS, Wet
  • Tensile Strength, ASTM D3039, Warp (0°), IM-7-6K-5HS
  • Tensile Strength, Fill (90°), IM-7-6K-5HS, Wet
  • Tensile Modulus, Fill (90°), IM-7-6K-5HS, Wet
  • Tensile Modulus, Warp (0°), IM-7-6K-5HS, Wet
  • Tensile Modulus, Open Hole, IM-7-6K-5HS
  • Tensile Modulus, Fill (90°), IM-7-6K-5HS, Wet
  • Tensile Modulus, Open Hole, IM-7-6K-5HS, Wet
  • Tensile Modulus, Warp (0°), IM-7-6K-5HS
  • Flexural Strength, Warp, (0°), IM7-6K-5HS, wet
  • Flexural Strength, Fill, (0°), IM7-6K-5HS, wet
  • Flexural Strength, Fill, (0°), IM7-6K-5HS
  • Flexural Strength, Warp, (0°), IM7-6K-5HS
  • Flexural Modulus, Fill, (0°), IM7-6K-5HS, wet
  • Flexural Modulus, Fill, (0°), IM7-6K-5HS
  • Flexural Modulus, Warp, (0°), IM7-6K-5HS
  • Flexural Modulus, Warp, (0°), IM7-6K-5HS, wet
  • Compressive Strength, Open Hole, [+,0,0,90,0] W/D=6, IM7-6K-5HS, wet
  • Compressive Strength, Open Hole, [+,0,0,90,0] W/D=6, IM7-6K-5HS, wet
  • Compressive Strength, Open Hole, [+,0,0,90,0] W/D=6, IM7-6K-5HS
  • Compressive Modulus, Open Hole, IM7-6K-5HS
  • Compressive Modulus, Open Hole, IM7-6K-5HS, wet
  • Shear Strength, ASTM D2344, Short Beam Warp (0°), IM7-6K-5HS, wet
  • Shear Strength, ASTM D2344, Short Beam Warp (0°), IM7-6K-5HS
  • Maximum Service Temperature, Air, Continuous; depends on cure cycle
  • Maximum Service Temperature, Air, short term; depends on cure cycle
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, QC-PT-22, Wet
  • Glass Transition Temp, Tg, Post Cure: 177°C for 6 hrs
  • Glass Transition Temp, Tg, Post Cure: 190°C for 6 hrs
  • Glass Transition Temp, Tg, Post Cure: 210°C for 6 hrs
  • Glass Transition Temp, Tg, Post Cure: 227°C for 6 hrs
  • Glass Transition Temp, Tg, QC-PT-22, Dry
  • Glass Transition Temp, Tg, Post Cure: 243°C for 6 hrs
  • Processing Temperature, Cure Temperature - Autoclave
  • Gel Time, QC-TP-87, in nitrogen atmosphere
  • Shelf Life
  • Shelf Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.