Promotor C is a promoter for cobalt-accelerated cure systems using ketone peroxides at ambient and elevated temperatures. CAS number: 123-54-6 EINECS/ELINCS No.204-634-0 Applications: Promotor C, acetylacetone or 2,4-pentanedione, is a promoter for ketone peroxide/cobalt accelerator based cure systems for the ambient and elevated temperature cure of unsaturated polyester resins.Promotor C when used in combination with e.g. Butanox M-50/ Accelerator NL-49PN will shorten the gel time and will increase the cure speed, which results in a shorter demoulding time.Promotor C can in this respect be used as an alternative for aromatic amines like Accelerator NL-63-10P. Promotor C will not give a yellow discoloration of the endproduct as observed with the use of an amine accelerator. Promotor C can very effectively be used at elevated temperatures to increase the reactivity of perester/cobalt accelerator based cure systems like Trigonox 21, Trigonox 42 or Trigonox C in combination with Accelerator NL-49PN (1% Cobalt) or Accelerator NL-51PN (6% Cobalt). Information provided by Nouryon |