Moplen RP210R is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP210R is a copolymer particularly suitable for extrusion coating and lamination of flexible film packaging. Moplen RP210R resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Low neck-in and high speed; Adhesion to OPP substrate; Heat seal performance Applications: Flexible film packaging (OPP) Information provided by PolyMirae Company Ltd. |