MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
The Chemical Company Edible grade Tartaric Acid, C4H6o6
Categories: Fluid

Material Notes: Tartaric Acid is a white crystalline diprotic organic acid. The compound occurs naturally in many plants, particularly in grapes, bananas, and tamarinds. It is also one of the main acids found in wine. Tartaric Acid can be added to food when a sour taste is desired. It is also used as an antioxidant. Salts of Tartaric Acid are known as tartarates. The chemical is a dihydroxy derivative of succinic acid. Tartaric Acid is found in cream of tartar and baking powder. The chemical compound is used in silvering mirrors, tanning leather, and in Rochelle Salt. In medical analysis, Tartaric Acid is used to make solutions for the determination of glucose.

Information provided by The Chemical Company

Key Words: diprotic
Vendors:
Available Properties
  • Particle Mesh Size, Granular-100%
  • Particle Mesh Size, Fine Granular< 99%
  • Particle Mesh Size, Granular< 10%
  • Particle Mesh Size, Fine Granular< 5%
  • Ash, sulfate ash
  • Arsenic, As
  • Lead, Pb, Heavy Metals (as Pb), 10ppm max
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.