MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Zell-Metall Engineering Plastics Zellamid 900 (POM-C)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Zellamid® 900 is the registered trademark of Zell-Metall’s high molecular weight Acetal resin.

Acetal (POM) is noted for it’s high mechanical strength, heat resistance and good antifriction properties. As water absorption is almost nil dimensional accuracy and stability is higher than that of nylons. Physical properties remain unchanged in various environments. This material is manufactured in natural - Zellamid® 900 and black color - Zellamid® 900 SW, using Copolymer resin. Homopolymer Acetal is available on special request. Typical applications are gears, levers, springs, snap connectors, cam switches, clamps, pump components, mud handling equipment, electronic and office machines . Acetal lends itself also to all submerged applications.

Vendors:
Available Properties
  • Density
  • Moisture Absorption at Equilibrium, ISO 1110; DIN 53714, 50% RH
  • Water Absorption at Saturation, ISO 62; DIN 53495, 23°C
  • Ball Indentation Hardness, ISO 2039; DIN 53456, H 358/30
  • Tensile Strength at Break, ISO 527; DIN 53455
  • Elongation at Break, ISO 527; DIN 53455
  • Tensile Modulus, ISO 527; DIN 53452
  • Charpy Impact Unnotched, ISO 179; DIN 53453
  • Charpy Impact Unnotched, ISO 179; DIN 53453
  • Volume Resistivity, IEC 167; DIN 53482
  • Dielectric Constant, IEC 250; DIN 53483
  • Dielectric Strength, IEC 243; DIN 53481
  • Dissipation Factor, IEC 250; DIN 53483
  • Comparative Tracking Index, IEC 112; DIN 53480, KB Method
  • CTE, linear, DIN 53752
  • Specific Heat Capacity, DIN 52612
  • Melting Point, ISO 1218 Method A; DIN 53736
  • Maximum Service Temperature, Air, IEC 216; DIN 53446, 20,000 hours; 50% Tensile Strength
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75; DIN 53461
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75; DIN 53461
  • Flammability, UL94
  • Flame Spread, VDE 0304T3, BH3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.