Description Chevron MC6560 is a high impact polystyrene injection molding material with well-balanced flow and set-up time and good resistance to heat distortion. It also has good impact strength at low temperatures and excellent chemical resistance. Chevron MC6560 natural complies with Food Additive Regulation 21CFR177.1640 for polystyrene and rubber modified polystyrene, which states that such materials may be safely used in contact with foods. Applications Chevron MC6560 is recommended for moldings with medium- to heavy-walled sections such as furniture, refrigerator breaker trim, housewares and appliances.Information provided by Chevron Phillips Chemical Company. The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008. |