MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Brewer Science BrewerBOND® 305 Temporary Bonding Material
Categories: Other Engineering Material

Material Notes: BrewerBOND® 305 temporary wafer bonding material is an organic coating that enables back-end-of-line (BEOL) processing of ultrathin wafers using standard semiconductor equipment. This product improves throughput, simplifies cleaning, and shortens processing time.

BrewerBOND® 305 material is an organic temporary bonding material that improves throughput, simplifies cleaning, and shortens processing time. The material is stable in back-end-of-line processing up to 300°C (depending on downstream process specifications). Debonding is efficient and can be done in two ways. The first method is laser debonding with no force. The second method is mechanical debonding at room temperature with low force. This debonding versatility makes BrewerBOND® 305 material a great option for many different wafer-processing needs.

Market sectors include 3-D wafer-level packaging; MEMS; and Compound semiconductor.

Benefits:

  • Enables backside temperature processing at 250°C - 300°C
  • Enables mechanical or laser debonding with low force
  • Maximizes wafer yield with optimized temporary wafer bonding with mechanical or laser debonding process
  • Post-bond TTV < 2 µm
  • Reduced cleaning chemical consumption and time

Information provided by Brewer Science.

Vendors:
Available Properties
  • Viscosity, Complex Melt Viscosity
  • Viscosity, Complex Melt Viscosity
  • Viscosity, Complex Melt Viscosity
  • Viscosity, Complex Melt Viscosity
  • Brookfield Viscosity, BrewerBOND® 305-30
  • Brookfield Viscosity, BrewerBOND® 305-30
  • Brookfield Viscosity, BrewerBOND® 305
  • Brookfield Viscosity, BrewerBOND® 305
  • Thickness, BrewerBOND® 305-30; Spin Speed 1700 rpm
  • Thickness, BrewerBOND® 305; Spin Speed 1700 rpm
  • Thickness, BrewerBOND® 305-30; Spin Speed 900 rpm
  • Thickness, BrewerBOND® 305; Spin Speed 900 rpm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.