MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative property also at low humidity. The surface resistance level of 109-1010 ohms can be achieved at 20-25 % dosing level (EOS/ESD S11.11-1993, IEC 61340-5-1). The let down ratio of the masterbatch with high impact polystyrene should be tested prior to its use with the polymer used in order to reach the desired dissipative level. The thickness of the outer layers can be thin (< 5%) depending on the extrusion line. With good processing the adhesion between the outer dissipative layer and the core layer is excellent. PRE-ELEC® ESD 6010 provides a clean solution for protecting the fragile electronics components. Because of the controlled ion content, the material can be used in clean room applications. PRE-ELEC® ESD 6010 should be diluted with extrusion grade high-impact polystyrene. The performace of ESD 6010 in coextrustion can further be improved by adding ~5% of SBS. This improves the ductility of the outer layer and the adnesion between the layers

Processing: PRE-ELEC® ESD 6010 / HIPS dry blend can be processed in normal processing conditions as with polystyrene.

Information from Premix OY

Vendors:
Available Properties
  • Density
  • Melt Flow
  • Surface Resistance, ISO IEC 61340-5-1, At 20-25% Dosing
  • Maximum Service Temperature, Air
  • Zone 1, Cylinder
  • Zone 1, Die
  • Zone 2, Cylinder
  • Zone 2, Die
  • Zone 3, Die
  • Zone 3, Cylinder
  • Zone 4, Die
  • Zone 4, Cylinder
  • Zone 5, Die
  • Zone 5, Cylinder
  • Roll Temperature, 3rd Roll
  • Roll Temperature, 1st Roll
  • Roll Temperature, 2nd Roll
  • Drying Temperature
  • Drying Temperature, Pre-drying in a dehumidifier
  • Dry Time
  • Dry Time
  • Moisture Content, when produced
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Premix Thermoplastics Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.