MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NOVA Chemicals SURPASS® CCs757-A sHDPE Injection Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes:

Bi-modal, Octene Copolymer

Features:

  • Excellent organoleptic properties that exceed brand owners' strict standards for water
  • Resin bi-modality enables exceptional processing characteristics and excellent stress cracking resistance
  • Outstanding stiffness that enables production of light weight caps
  • Fully recyclable

Additives:

  • Processing antioxidant

Applications:

  • Injection molded caps and closures for still and sparkling water

United States: SURPASS CCs757-A resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors:
Available Properties
  • Density, ASTM D 792
  • ESCR 100% Igepal®, ASTM D 1693, F50, Condition B
  • Melt Index of Compound, ASTM D 1238
  • Hardness, Shore D, ASTM D 2240
  • Tensile Strength, ASTM D 638
  • Tensile Strength, Yield, Tensile pull speed 50 mm/min.
  • Elongation at Break, ASTM D 638, Tensile pull speed 50 mm/min
  • Elongation at Yield, ASTM D 638, Tensile pull speed 50 mm/min
  • Flexural Modulus, ASTM D 882, Procedure B
  • Flexural Modulus, 1% Secant, ASTM D 790, Procedure B
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.