MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Titanium Grade 4
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Information provided by Allvac and the references.

Characteristics: Intermediate strength, good weldability, suitable for cold forming and hot forming

Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets, fire walls, shrouds and tail pipes for jet engines.

Forms typically available: billet, bar, plate, sheet, strip, rod, wire, extrusions, tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: ASTM Grade 4: UNS R50700, CP titanium, C.P. titanium alloy
Vendors:
Available Properties
  • Density
  • Thermal Neutron Cross Section, Naturally occurring Ti
  • Hardness, Brinell, annealed
  • Hardness, Knoop, unwelded sheet
  • Hardness, Rockwell B, unwelded sheet
  • Hardness, Rockwell B, annealed
  • Hardness, Rockwell C, Estimated from Brinell.
  • Hardness, Vickers, Estimated from Brinell.
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength, Yield
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Elongation at Break, in 50 mm
  • Elongation at Break
  • Reduction of Area
  • Tensile Modulus
  • Tensile Modulus
  • Tensile Modulus
  • Tensile Modulus
  • Tensile Modulus
  • Tensile Modulus
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Modulus
  • Ultimate Bearing Strength
  • Ultimate Bearing Strength
  • Ultimate Bearing Strength
  • Ultimate Bearing Strength
  • Ultimate Bearing Strength
  • Ultimate Bearing Strength
  • Bearing Yield Strength, 2% permanent set.
  • Bearing Yield Strength, 2% permanent set.
  • Bearing Yield Strength, 2% permanent set.
  • Bearing Yield Strength, 2% permanent set.
  • Bearing Yield Strength, 2% permanent set.
  • Bearing Yield Strength, 2% permanent set.
  • Poissons Ratio
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength, Kt (stress concentration factor) = 2.7
  • Fatigue Strength, Kt (stress concentration factor) = 2.7
  • Fatigue Strength, unnotched
  • Fatigue Strength, Unnotched
  • Fracture Toughness, for K(Q) annealed
  • Shear Modulus
  • Shear Modulus
  • Shear Modulus
  • Shear Modulus
  • Shear Modulus
  • Shear Modulus
  • Shear Modulus
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Charpy Impact, Notched
  • Charpy Impact, Notched
  • Charpy Impact, Notched
  • Charpy Impact, Notched
  • Coefficient of Friction, Dynamic, Ti sliding on Ti; 300 m/min
  • Coefficient of Friction, Dynamic, Ti sliding on Ti; 40 m/min
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Magnetic Permeability, at 1.6 kA/m
  • Heat of Fusion, High Purity Ti.
  • CTE, linear
  • CTE, linear, average
  • CTE, linear, perpendicular to the c-axis
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Liquidus
  • Beta Transus
  • Emissivity (0-1), High purity Ti
  • Reflection Coefficient, Visible (0-1), High purity Ti; visible light.
  • Carbon, C
  • Hydrogen, H
  • Iron, Fe
  • Nitrogen, N
  • Other, each
  • Other, total
  • Oxygen, O
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.