MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Mitsubishi Chemical Advanced Materials Nylatron® 66 SA FR PA66 Nylon 66, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Nylatron® 66 SA Flame Retardant (FR) Polyamide PA66 shapes were developed to fulfill the requirements of the plastic flammability test, which determines the tendency of the material to either extinguish or spread the flame once the it has been ignited. This test procedure is described in UL 94, and this particular Nylatron® grade fulfills the V-0 criteria from a thickness of 1 mm, while also meeting the requirements of EN 45545-2 regulation- a standard specific to railway applications. For these reasons, Nylatron® SA FR PA66 components are often favored solutions for applications within the transportation and railway markets such as, cable holders, clamps, and channels, and connections / sockets.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183-1
  • Water Absorption, ASTM D570, immersion in water
  • Water Absorption at Saturation, ASTM D570
  • Hardness, Rockwell M, ISO 2039-2
  • Tensile Strength, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Yield, ISO 527-1/-2
  • Modulus of Elasticity, ISO 527-1/-2
  • Compressive Strength, ISO 604
  • Compressive Strength, ISO 604
  • Compressive Strength, ISO 604
  • Charpy Impact Unnotched, ISO 179-1/1eU
  • Charpy Impact, Notched, ISO 179-1/1eA
  • Surface Resistivity per Square, ANSI/ESD STM 11.11
  • Dielectric Strength, IEC 60243-1
  • CTE, linear
  • Melting Point, ISO 11357-1/-3, 10°C / min
  • Maximum Service Temperature, Air, 20,000 hours
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index, ISO 4589-1/-2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Mitsubishi Chemical Advanced Materials (former Quadrant Engineering Plastics Products)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.