MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Alfa Chemistry Materials Zinc stearate
Material Notes: Applications: It is widely used as a release agent for the production of many kinds of objects rubber, poly urethane, polyester processing system, powder metallurgy. These applications exploit its "non-stick" properties . In cosmetics, zinc stearate is a lubricant and thickening to improve texture. It is an "activator" for rubber vulcanization by sulfur and accelerators. As discovered in the early days of vulcanization, zinc has a beneficial effect on the reaction of the sulfur with the polyolefin. The stearate is a form of zinc that is highly soluble in the nonpolar medium of the poly olefins. Being lipophilic, it functions as a phase transfer catalyst for the saponification of fats. Zinc stearate is used in cosmetic formulations to increase adhesive properties. It is also used as a coloring agent. This is a mixture of the zinc salts of stearic and palmitic acids. Zinc stearate is primarily used in pharmaceutical formulations as a lubricant in tablet and capsule manufacture at concentrations up to 1.5% w/w. It has also been used as a thickening and opacifying agent in cosmetic and pharmaceutical creams, and as a dusting powder.

ZINC STEARATE is a white, hydrophobic powder with a slight, characteristic odor. Insoluble in water, ethyl alcohol and diethyl ether. Soluble in acids. Non-toxic. In technical grades, the percentage of zinc may vary according to the intended use. Products with less than the theoretical amount of zinc are more acidic.

Synonyms: Zinc distearate; Zn Stearate; Zincum stearinicum; Zink distearat; Octadecanoic acid, zinc salt; UNII-H92E6QA4FV; A830766; XOOUIPVCVHRTMJ-UHFFFAOYSA-L; Stearic acid, zinc salt;

Smiles: CCCCCCCCCCCCCCCCCC(=O)[O-].CCCCCCCCCCCCCCCCCC(=O)[O-].[Zn+2];

Information provided by Alfa Chemistry Materials.

Vendors:
Available Properties
  • Density
  • Molecular Weight, "Exact Mass" - Based on Specific Isotopes
  • Molecular Weight, Monoisotopic Mass - Isotopic Peak from Most Abundant Isotopes
  • Molecular Weight
  • Vapor Pressure
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.