MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
AGC AFLAS® PM-3000 TFE/P Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: AFLAS® FFKM Series is a new perfluoroelastomer product line classified as an FFKM. AFLAS PM-3000 is a semi-commercialized elastomer having the chemical structure derived from tetrafluoroethylene and perfluoroalkylvinylether. This chemical structure offers outstanding resistance to chemicals, oils, solvents, and more. PM-3000 is a peroxide-curable perfluoroelatomer.

Material Features:

  • Outstanding chemical resistance
  • Superior oil resistance
  • Outstanding solvent resistance
  • Excellent heat resistance
  • Excellent compression set
  • Exceptional mechanical strength
  • Excellent processability
End User Benefits:
  • Highly suitable for extremely harsh and aggressive chemical environments
  • Hot service temperature at 250°C, with peak exposure of 270°C
  • Can be compounded to be highly resistant to rapid gas decompression (e.g. NORSOK)
Typical Applications:
  • O-rings
  • Gaskets
  • Oilfield parts
  • Semiconductor parts

Information provided by AGC Chemicals Americas Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Mooney Viscosity, ML1+4
  • Hardness, Shore A
  • Hardness, Shore A, Heat Resistance
  • Hardness, Shore A, Heat Resistance
  • Hardness, Shore A, Heat Resistance
  • Tensile Strength
  • Tensile Strength, Heat Resistance
  • Tensile Strength, Heat Resistance
  • Tensile Strength, Heat Resistance
  • Elongation at Break
  • Elongation at Break, Heat Resistance
  • Elongation at Break, Heat Resistance
  • Elongation at Break, Heat Resistance
  • Tensile Modulus, Storage Modulus
  • 100% Modulus
  • Compression Set, ASTM-type 1 button
  • Compression Set, O-ring
  • Compression Set, O-ring
  • Compression Set, O-ring
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Air, peak
  • Cure Time, 10% Cure, 100CPM, 3° Strain, 12 minutes by RPA-2000
  • Cure Time, 90% Cure, 100CPM, 3° Strain, 12 minutes by RPA-2000
  • Cure Time, Press cure
  • Cure Time, Post cure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Asahi Glass Company, AGC Fluorocompounds

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.