MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Teknor Apex SarlinkĀ® TPV X4750B42 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 4700 Series are a very high flow injection molded engineering grades with excellent UV resistance, elasticity, and surface aesthetics designed for demanding automotive applications including window encapsulation and exterior parts. This product is a black, medium hardness, low density thermoplastic vulcanizate suited for injection molding applications that require superior flow properties.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Processability; High Flow; High Heat Resistance; Low Compression Set; Low Density; Low Specific Gravity; Medium Hardness; Resilient; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Automotive Specifications: CHRYSLER MS-AR-100 AMV Color: Natural; GM GMP.E/P.078 Color: Natural; GM GMW15812P-TPV (EPDM=PP) Type 4M Color: Natural; GM Sarlink Color

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity, ASTM D3835, Shear, Capillary
  • Hardness, Shore A, ISO 868, Extruded
  • Hardness, Shore A, ISO 868, Injection Molded
  • Tensile Strength at Break, ISO 37, Flow
  • Tensile Strength at Break, ISO 37, Across Flow
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air at 168 hr
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air at 168 hr
  • Tensile Stress at Strain, ISO 37, Across Flow
  • Tensile Stress at Strain, ISO 37, Flow
  • Tensile Stress at Strain, ISO 188, Across Flow, Change in Air at 168 hr
  • Tensile Stress at Strain, ISO 188, Across Flow, Change in Air at 1000 hr
  • Elongation at Break, ISO 37, Flow
  • Elongation at Break, ISO 37, Across Flow
  • Elongation at Break, ISO 188, Across Flow, Change in Air at 168 hr
  • Elongation at Break, ISO 188, Across Flow, Change in Air at 168 hr
  • Tear Strength, ISO 34-1, Method Ba, Angle (Unnicked)
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Processing Temperature, Injection, Melt
  • Rear Barrel Temperature, Injection
  • Middle Barrel Temperature, Injection
  • Front Barrel Temperature, Injection
  • Nozzle Temperature, Injection
  • Mold Temperature, Injection
  • Drying Temperature
  • Dry Time
  • Back Pressure, Injection
  • Screw Speed, Injection
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.