Comments: Low Viscosity, Index Matches BK7, Glass Use with Phosphor, Index matches to plastic such as COC
Applications: Excellent for LC D D isplay and LED Encapsulation
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic