MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Sandvik 19.9.L CRYO Welding Wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.9.L CRYO is a filler material for joining austenitic stainless steels, e.g. ASTM 304, 304L (18Cr/8Ni/ELC), for cryogenic applications and meets the requirements of ASME Section VIII, Division 1, UHA 51 ((a) (4) (-a) (-1)) and others. It is also used for service temperatures down to 269°C (-452°F), and ferritic or martensitic stainless steels with maximum 19% Cr. Sandvik 19.9.L Cryo is approved by TÜV Rheinland for use at cryogenic temperatures down to 4K (-269°C (-452°F)). It is suitable for joining stainless steels of 18Cr/8Ni/Nb types, e.g. ASTM 347, for service temperatures up to 350°C (660°F). Sandvik 19.9.L CRYO is available as wire and rods for MIG/MAG, TIG, plasma arc, and submerged arc welding (SAW). Specifically developed for welding in cryogenic applications, typically: manufacturing of dewars, containers, tanks, cryostats, and transfer systems for transportation and storage of LNG, LPG, liquid nitrogen and liquid helium. The chemical composition is optimized for cryogenic applications in terms of impact strength and other characteristics. It has a controlled chemical composition and ferrite content for resistance to microfissuring, and balanced minor additions of certain elements for optimum arc stability, fluidity and low spatter.

Information provided by Sandvik

Vendors:
Available Properties
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, SAW - typical for non-heat treated weld metal using flux 15W
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield, SAW - typical for non-heat treated weld metal using flux 15W
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Break, SAW - typical for non-heat treated weld metal using flux 15W
  • Elongation at Break
  • Reduction of Area
  • Charpy Impact
  • Charpy Impact, SAW - typical for non-heat treated weld metal using flux 15W
  • Charpy Impact
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Minimum Service Temperature, Air
  • Carbon, C, welding with a shielding gas of Ar + 2%O2
  • Carbon, C, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Carbon, C
  • Chromium, Cr, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Chromium, Cr
  • Chromium, Cr, welding with a shielding gas of Ar + 2%O2
  • Manganese, Mn, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Manganese, Mn, welding with a shielding gas of Ar + 2%O2
  • Manganese, Mn
  • Molybdenum, Mo, welding with a shielding gas of Ar + 2%O2
  • Molybdenum, Mo, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Molybdenum, Mo
  • Nickel, Ni, welding with a shielding gas of Ar + 2%O2
  • Nickel, Ni, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Nickel, Ni
  • Nitrogen, N, welding with a shielding gas of Ar + 2%O2
  • Nitrogen, N, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Nitrogen, N
  • Phosphorus, P, welding with a shielding gas of Ar + 2%O2
  • Phosphorus, P, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Phosphorus, P
  • Silicon, Si, welding with a shielding gas of Ar + 2%O2
  • Silicon, Si
  • Silicon, Si, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Sulfur, S, welding with a shielding gas of Ar + 2%O2
  • Sulfur, S, non-heat treated all weld metal made by SAW, Flux 15W/35W
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.