MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Bisalloy Steels BisPlate 80 Thickness >80-100 mm
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the high strength properties of BISPLATE 80 allows reduction in section thickness without loss of structural integrity.

Applications: Transport Equipment, High Rise Buildings, Bridges, Excavator Buckets, Storage Tanks, Lifting Equipment, Mining Equipment, Induced Draft Fans

Testing: AS/NZS 3597 Grade 700 NATA approved

Welding: According to AS/NZS 1554 parts 4 and 5

Tolerance: In accordance with AS/NZS 1365

Key Words: ASTM A514, ISO 4950-3 Grade E690, ISO 9328-4 Grade P690TQ, EN 10137-2 Grade S690Q, JIS G3128
Vendors:
Available Properties
  • Hardness, Brinell
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break, in 50 mm GL
  • Charpy Impact, Longitudinal
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.