MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes:

Features:

  • Moderate toughness and strength
  • Good stiffness
  • Easy processability
  • Excellent seal properties
  • Applications:

  • Heavy duty shipping sacks requiring moderate toughness and high stiffness
  • Industrial packaging
  • Industrial liners
  • Construction films
  • Automatic packaging film
  • Information provided by Nova Chemicals

    Vendors:
    Available Properties
    • Density, ASTM D792
    • Thickness
    • Thickness
    • Melt Flow, ASTM D1238
    • Tensile Strength, Yield, ASTM D882, MD, 1 mil
    • Tensile Strength, Yield, ASTM D882, TD, 1 mil
    • Tensile Strength, Yield, ASTM D882, TD, 3 mil
    • Tensile Strength, Yield, ASTM D882, MD, 3 mil
    • Elongation at Break, ASTM D638, MD, 1 mil
    • Elongation at Break, ASTM D882, MD, 3 mil
    • Elongation at Break, ASTM D882, TD, 3 mil
    • Elongation at Break, ASTM D882, TD, 1 mil
    • Puncture Energy, Low Friction Puncture
    • Elmendorf Tear Strength MD, ASTM D1922, 1 mil
    • Elmendorf Tear Strength MD, ASTM D1922, 3 mil
    • Elmendorf Tear Strength TD, ASTM D1922, 1 mil
    • Elmendorf Tear Strength TD, ASTM D1922, 3 mil
    • Dart Drop Test, ASTM D1709/A, 1 mil
    • Dart Drop Test, ASTM D1709/A, 3 mil
    • Film Tensile Strength at Break, MD, ASTM D882, 3 mil
    • Film Tensile Strength at Break, MD, ASTM D882, 1 mil
    • Film Tensile Strength at Break, TD, ASTM D882, 1 mil
    • Film Tensile Strength at Break, TD, ASTM D882, 3 mil
    • 1% Secant Modulus, MD, ASTM D882, 3 mil
    • 1% Secant Modulus, MD, ASTM D882, 1 mil
    • 1% Secant Modulus, TD, ASTM D882, 1 mil
    • 1% Secant Modulus, TD, ASTM D882, 3 mil
    • Haze, ASTM D1003
    • Haze, ASTM D1003
    • Gloss, ASTM D2457, 1 mil, at 45°
    • Gloss, ASTM D2457, 3 mil, at 45°
    • Melt Temperature
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.