MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Röchling GLASGUARD 1130 Corrosion-Resistant Panels
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: GlasGuard Grade 1130 is a fiberglass-reinforced thermoset polymer composite system which is available as sheet stock or in a variety of pultruded shapes. Grade 1130 possesses flame resistance, corrosion resistance, weatherability, and dielectric properties. This material meets NEMA criteria for grade GPO-3. Grade 1130 was developed to meet the requirements of the NYC Transit Authority. It has been pultruded into channel shaped covers for the electrified third rail and molded into flat panels for both a sign material and switchgear components.

Information provided by Glastic Corporation

Vendors:
Available Properties
  • Water Absorption, ASTM D-570, % by wt.
  • Tensile Strength, Yield, ASTM D-638, Lengthwise
  • Tensile Strength, Yield, ASTM D-638, Crosswise
  • Tensile Modulus, ASTM D-638, Lengthwise/Crosswise
  • Flexural Strength, ASTM D-790, Lengthwise
  • Flexural Strength, ASTM D-790, Crosswise
  • Flexural Modulus, ASTM D-790, Crosswise
  • Flexural Modulus, ASTM D-790, Lengthwise
  • Adhesive Bond Strength, NEMA 11.11, lbs.
  • Izod Impact, Notched, ASTM D-256
  • Dielectric Strength, ASTM D-149, Perpendicular S/T in Air
  • Arc Resistance, ASTM D-495
  • Track Resistance, ASTM D-2303, Inclined Plane
  • Flammability, UL94
  • Flame Spread Index, ASTM E-162, Radiant Panel
  • Flame Spread Index, ASTM E-84, UL Standard 723
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.