RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion temperature (HDT). This grade is formulated with UV absorber, which protects the contents from UV radiation. This grade also features high heat distortion temperature. Applications: industrial chemicals, household and chemical containers such as detergents, cleaners, motor oils, and cosmetics.Information provided by Borealis AG |