MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Momentive Performance Materials GE Sealants & Adhesives Advanced Silicone 2 Window & Door Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Advanced Silicone 2 Window & Door sealant is 100% waterproof and can be exposed to rain or water in as little as 30 minutes. It is ideal for weatherproofing and application on a wide range of projects exposed to harsh weather conditions. This high-performance sealant is permanently flexible, shrink proof, crack-proof, and offers strong adhesion to many common substrates. It has 10-year mold free product protection, is low in odor, and will not blemish most metal finishes. From new construction to renovations, window and door installations to general weather sealing, versatile and proven Advanced Silicone 2 Window & Door sealant offers a durable yet highly flexible seal. Backed by a lifetime guarantee.

Features: Meets ASTM C-920 Class 35 specifications, 40% more flexibility than Class 25 sealants, 5X stronger adhesion, 30-minute rain & water ready, 100% silicone is 100% waterproof and 100% weatherproof, Resist mold with 10-year mold-free product protection, Will not blemish most high-end metal finishes such as chrome, bronze and nickel, Will not break down due to extreme weather conditions, freeze & sun-proof, Shrink & crack-proof, Excellent adhesion for wet or dry surface applications, Freeze/thaw stability, Non-paintable.

Applications: Advanced Silicone 2* Window & Door sealant is used in a wide variety of applications including windows, doors, siding, trim, vents, asphalt, cement, brick, mortar, and attic/basement applications.

Information provided by Momentive Performance Materials.

Vendors:
Available Properties
  • Specific Gravity, Cured.
  • Volatile Organic Compounds (VOC) Content, WPSTM C1454, Uncured. Excluding water & exempt compounds
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Full Cure
  • Tack-Free Time, ASTM C679, 50% RH
  • Working Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Momentive Performance Materials (GE Silicones)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.