MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Bohler-Uddeholm UDDEHOLM Caldie Plastic Mold Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Description: Uddeholm Caldie is a chromium-molybdenumvanadium alloyed tool steel.
    Uddeholm Caldie which is characterized by:
  • Very good chipping and cracking resistance
  • Good wear resistance
  • High hardness (>60 HRC) after high temperature tempering
  • Good dimensional stability in heat treatment and in service
  • Excellent through-hardening properties
  • Good machinability and grindability
  • Excellent polishability
  • Good surface treatment properties
  • Good resistance to tempering back
  • Very good WEDM properties
Applications: Uddeholm Caldie is suitable for short to medium run tooling where chipping and/or cracking are the predominant failure mechanisms and where a high compressive strength (hardness of over 60 HRC) is necessary. This makes Uddeholm Caldie an excellent problem solver for severe cold work applications where the combination of a hardness above 60 HRC and a high cracking resistance is of utmost importance e.g. as in the blanking and forming of ultra high strength steel sheets. Uddeholm Caldie is also very suitable as a substrate steel for applications where surface coatings are desirable or necessary
    Cold Work Applications:
  • Blanking applications where high ductility and toughness are needed to prevent chipping/cracking
  • Cold forging and forming operations where a high compressive strength combined with good resistance to chipping/cracking are necessary
  • Machine knives
  • Thread rolling dies
  • Substrate for surface coatings

Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Soft annealed
  • Hardness, Rockwell C, typical range of use after hardening/tempering
  • Modulus of Elasticity, Hardened and tempered to 60-62 HRC
  • Modulus of Elasticity, Hardened and tempered to 60-62 HRC
  • Modulus of Elasticity, Hardened and tempered to 60-62 HRC
  • Compressive Strength, Rc0.2; varies with tempering. This range is for HRC between 58 and 61.
  • CTE, linear, Hardened and tempered to 60-62 HRC
  • CTE, linear, Hardened and tempered to 60-62 HRC
  • Specific Heat Capacity, Hardened and tempered to 60-62 HRC
  • Thermal Conductivity, Hardened and tempered to 60-62 HRC
  • Thermal Conductivity, Hardened and tempered to 60-62 HRC
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.