Features: Modified homopolymer PP for injection moulding, chemically reinforced with 60% glass fibre, contains the modifier of mechanical properties.Very good strength and tensile modulus. Delivered in natural mode and in the full RAL colour scale. Packaging, transport, stocking: The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation. Information Provided by Plastcom spol. s r.o. |