MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Covestro Makrolon® DX-NR sheet Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Polycarbonate diffuser sheet for outdoor LED lighting Makrolon DX-NR is a translucent polycarbonate product specifically designed for use as a lighting lens in outdoor applications. The diffuser technology helps to provide uniform luminance and ensures elimination of LED hot spots while maintaining high light transmission. The advanced UV resistance technology provides long lasting weathering performance and the non-reflective texture built into the UV resistant side of the sheet, enhances its aesthetics. When compared to other light diffusing products such as glass and acrylic, Makrolon DX-NR has superior impact strength and toughness. Its higher flammability resistance and wider service temperature provide an additional advantage over acrylic diffusers.

Information provided by Covestro

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Poissons Ratio, ASTM E132
  • Impact Test, ASTM D3763
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D 150
  • Dielectric Constant, ASTM D 150
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  • Flammability, UL94
  • Glow Wire Ignition Temperature, DIN EN 60695-2-13
  • Glow Wire Flammability Index, DIN EN 60695-2-12
  • Transmission, Visible, ASTM D1003
  • Transmission, Visible, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.