MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Kohesi Bond KB 1823 HTND One part, heat curing epoxy for bonding, sealing and coating
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Highlights:
  • Superior tensile lap shear strength
  • Non drip property
  • service up to 260°C
  • Outstanding chemical resistance
  • Superb electrical insulator
  • Very high Tg (~ 158°C)
Kohesi Bond KB 1823 HTND is a true single component system that requires no mixing and cures hard at elevated temperatures. It readily cures at 150°C - 180°C for a period of 60 - 90 minutes. For optimum performance, a post cure for 2 hours at 180°C - 200° is highly recommended. This product has a slightly exothermic cure and it is recommended to cure it in bond line thickness of 2-8 mils. KB 1823 HTND offers an extensive service temperature range of -50°C to +260°C. It is primarily used a structural adhesive owing to its first-rate dimensional stability, tensile lap shear strength and compressive strength. KB 1823 HTND offers a non-drip paste consistency that will not flow even during cure. Being a one component system, it provides ease of application and also adheres well to a broad variety of substrates including metals, ceramics, most plastics and glass. KB 1823 HTND is a 100% solids and a reactive system i.e. it does not contain any solvents or diluents. In addition to superior electrical insulation, KB 1823 HTND also offers excellent chemical resistance to a variety of acids, bases, fuels, oils and water. It has a gray color. With a combination of Excellent structural bonding, ease of use and handling, KB 1823 HTND is universally used in electronics, aerospace, specialty OEM and various other industries.

Typical Applications:

  • Bonding
  • Sealing

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Hardness, Shore D
  • Tensile Strength
  • Compressive Strength
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time, Optimum post cure
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.