MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metalmen Sales
Haynes Hastelloy® C-276 alloy, solution heat treated flat products
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn't need to be solution heat-treated after welding and has vastly improved fabricability. This alloy resists the formation of grain-boundary precipitates in the weld heat-affected zone, thus making it suitable for most chemical process applications in the as-welded condition. However, in environments where attack of the C-276 alloy weld joint is experienced. C-22® weld filler materials should be considered. C-276 alloy has excellent resistance to localized corrosion and to both oxidizing and reducing media. Because of its versatility, C-276 alloy can be used where "upset" conditions are likely to occur or in multipurpose plants.

Hastelloy C-276 alloy excellent resistance to a wide variety of chemical process environments, including strong oxidizers such as ferric and cupric chlorides, hot contaminated media (organic and inorganic), chlorine, formic and acetic acids, acetic anhydride, and seawater and brine solutions. It is used in flue gas desulfurizations systems because of its excellent resistance to sulfur compounds and chloride ions encountered in most scrubbers. C-276 alloy has excellent resistance to pitting and to stress- corrosion cracking. It is also one of the few materials that withstands the corrosive effects of wet chlorine gas, hypochlorite, and chlorine dioxide.

Hastelloy C-276 alloy can be forged, hot-upset, and impact extruded. Although the alloy tends to work-harden, it can be successfully deep-drawn, spun, press formed or punched. All of the common methods of welding can be used to weld Hastelloy C-276 alloy, although the oxyacetylene process is not recommended. Special precautions should be taken to avoid excessive heat input.

Hastelloy C-276 is available in the form of plate, sheet, strip, billet, bar, wire, covered electrodes, pipe, tubing, pipe fittings, flanges, fittings.

Heat Treatment: C-276 alloy is normally solution heat-treated at 2050°F (1121°C) and rapid quenched. If possible, parts which have been hot-formed should be solution heat-treated prior to final fabrication or installation.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: UNS N10276, ASME SB-574, ASME SB-575, ASME SB-619, ASME SB-622, and ASME SB-626
Vendors:
Available Properties
  • Density, at RT
  • Hardness, Rockwell B, plate
  • Hardness, Rockwell B, sheet
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Tensile Strength, Yield, 0.2% offset
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Elongation at Break, in 50.8 mm
  • Modulus of Elasticity, RT
  • Modulus of Elasticity, heat treated at 1121°C (2050°F) and rapid quenched
  • Modulus of Elasticity, heat treated at 1121°C (2050°F) and rapid quenched
  • Modulus of Elasticity, heat treated at 1121°C (2050°F) and rapid quenched
  • Modulus of Elasticity, heat treated at 1121°C (2050°F) and rapid quenched
  • Charpy Impact, V Notch; plate; aged 1000 hours at 538°C (1000°F)
  • Charpy Impact, V Notch; plate; aged 100 hours at 538°C (1000°F)
  • Charpy Impact, V Notch; plate; aged 100 hours at 260°C
  • Charpy Impact, V Notch; plate; solution heat treated at 1121°C (2050°F), rapid quenched
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity, RT
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Tungsten, W
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Haynes International, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.