MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Master Bond EP45HTND-2 Chemically Resistant, Non-Drip Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond EP45HTND-2 is a two component epoxy system for high performance bonding, sealing and coating. It is used for applications requiring solid temperature resistance and capable of withstanding aggressive chemicals. In fact, it is formulated to resist many of these chemicals even at elevated temperatures. EP45HTND-2 has a 100 to 30 mix ratio by weight. It contains no solvents or diluents, has a very smooth paste-like consistency as well as a very long open time. The system requires oven curing at 250-300°F for 3-4 hours. The optimal cure schedule is more of a ramp up type cure, that being 30-60 minutes at 200°F, 1 hour at 250°F and 2-3 hours at 300°F, followed by a post cure of 1-2 hours at 350°F. EP45HTND-2 will not flow or run when curing. It bonds well to metals, glass, ceramics, rubber and many plastics. The service temperature range is -80°F to +500°F. It is especially effective against aggressive chemicals particularly those found in downhole applications as well as many potent acids, bases and solvents. It is an outstanding electrical insulator with excellent physical strength properties. Both Parts A and B are colored amber. This versatile system is widely used in oil well, aerospace, electronic, specialty OEM and related applications where the cured properties mentioned above are needed and the material will stay in place while curing.

Product Advantages:

  • Easy to apply; paste viscosity; spreads evenly and smoothly.
  • Exceptionally long working life at room temperature.
  • Outstanding adhesion to a wide variety of substrates.
  • Highly resistant to many chemicals especially those in petroleum products.
  • Remarkable temperature resistance from -80°F to +500°F.
  • Fine physical strength property profile.
Key Features:
  • Non-drip paste consistency
  • Will not flow when curing
  • Outstanding chemical resistance
  • Serviceable from -80°F to +500°F

Information provided by MasterBond®

Vendors:
Available Properties
  • Hardness, Shore D
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Modulus
  • Shear Strength, Tensile lap, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time, 1 hour at 250°F and 2-3 hours at 300°F, plus a post cure of 1-2 hours at 350°F
  • Cure Time
  • Pot Life, 100 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.