Soft and flexible, Tygon® E-1000 Non-DEHP laboratory tubing delivers the same performance in a formulation that contains non-DEHP [Bis (2-ethylhexyl) phthalate] plasticizers. The market demand and certain global and regional requirements such as Europe's REACH, EU food directives and California Prop 65 motivated Saint-Gobain to develop tubing products that contain a globally accepted substitute for DEHP. Tygon E-1000 Non-DEHP laboratory tubing has been tested rigorously to ensure that it meets the same physical standards, including low temperature and corrosive chemical resistance as the old Tygon® R-1000 tubing. Tygon® E-1000 tubing stays flexible at temperatures as low as -67°F (-55°C ). Its smooth bore facilitates easy cleaning and helps prevent possible buildup. Do not autoclave. Features and Benefits - Ultra-soft and flexible
- Performs well at low temperatures (to -67°F)
- Excellent for use in low-torque pump application
Regulatory Information: This product complies with NSF 51 and FDA requirements. Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM placques or molded ASTM durometer buttons. Information provided by Saint Gobain Performance Products. |