MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Wefapress St 7000® FRAS PE-UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: The premium quality St 7000® FRAS (fire-resistant and antistatic) is used in areas in which special fire regulations and electrostatic properties have to be fulfilled. With a surface resistance of < 10^7 ?, the material, based on ultra-high molecular weight polyethylene (PE-UHMW), displays good conductivity. Special additives additionally ensure flame-retarding behavior. In fire hazard testing conducted in accordance with DIN EN 60695-11-10:1999, St 7000® FRAS was rated in the classed HB40 (HB = horizontal burn) and V-0 (V = vertical burn). Properties: Anti-static, Flame retardant, High wear resistance, Zero moisture absorption, Excellent impact resistance.

Applications: Guide rails, Sliding profiles, slide bearings, slide rails, Shock and impact resistant parts. Industries: Conveyor systems and automation, Mechanical and plant engineering.

Information provided by Wefapress.

Vendors:
Available Properties
  • Density, DIN 53479
  • Moisture Absorption
  • Molecular Weight
  • Hardness, Shore D, DIN 53505
  • Ball Indentation Hardness, DIN ISO 2039 Teil 1
  • Elongation at Break, DIN ISO / R 527
  • Modulus of Elasticity, DIN 53457
  • Charpy Impact, Notched, DIN 53457
  • Coefficient of Friction
  • Sand Slurry, % Abrasion
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • CTE, linear, DIN ISO 11359
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, DTA
  • Maximum Service Temperature, Air, Continuous Application Temp.
  • Vicat Softening Point, DIN 53460
  • Minimum Service Temperature, Air
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.