MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Syensqo (Solvay Specialty Polymers) KetaSpire® XT-920 GF30 PEEK, 30% glass fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: KetaSpire® XT-920 GF30 is a 30% glass fiber reinforced, natural color grade of the industry's first true a high-temperature PEEK. Glass fiber reinforcement provides higher strength and stiffness properties than unreinforced KetaSpire® XT-920 resin, making it suitable for structural applications needing robust mechanical properties, particularly those with service temperatures approaching 300°C.

The PEEK designation is based on the 2:1 ratio of ether-to-ketone functional groups in the polymer backbone. The material provides the exceptional chemical resistance of PEEK along with a 20°C (36°F) higher glass transition temperature and a 45°C (81°F) higher melting temperature than standard PEEK. This increase in thermal performance allows engineers to achieve higher mechanical strength for components used in higher temperature and higher pressure operating environments.

Although other high-temperature polyketones exhibit thermal properties on par with KetaSpire® XT, their chemical resistance is significantly inferior to standard PEEK and KetaSpire® XT. The material's unique combination of properties makes KetaSpire® XT well-suited for applications in oil & gas, transportation, electronics, chemical processing, and other industrial uses.

Applications: Aircraft Applications; Automotive Applications; Connectors; Electrical/Electronic Applications; Housings; Industrial Applications; Oil/Gas Applications; Pump Parts; Seals

Features: Chemical Resistant; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; High Heat Resistance; Radiotranslucent; Steam Resistant

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Viscosity, ASTM D3835, Melt
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell M, ASTM D785
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638, 5.0 mm/min
  • Tensile Strength at Break, ISO 527-2, Type 1A, 5 mm/min
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ASTM D638, 5.0 mm/min
  • Tensile Modulus, ASTM D638, 5.0 mm/min
  • Tensile Modulus, ISO 527-2, Type 1A
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Compressive Strength, ASTM D695
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Unnotched (ISO), ISO 180
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, Parallel to Flow, ASTM E831
  • Melting Point, ASTM D3418, Peak
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Glass Transition Temp, Tg, DSC
  • Flammability, UL94
  • Flammability, UL94
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.