MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
LG Chemical NBR 8300 High Acrylonitrile Polymer  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: NBR 8300 is a copolymer of butadiene-acrylonitrile and the powdered nitrile elastomer manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 8300 has excellent compatibility with up to 100 parts of PVC resin, its plasticizers, fillers, heat/UV stabilizers and pigments. Within a PVC matrix, NBR 8300 adds the oil and fuel resistance to PVC compound and also it can improve the impact resistance of PVC. NBR 8300/PVC blend acts like a TPEs and substitutes for vulcanized rubber and TPU in many applications due to its excellent fuel and grease resistance.

Applications: NBR 8300 is recommended to use in overflow tubing, vacuum tubing, grommet seals, cable sleeves, gaiters, guard bellows, fuel hoses and seals. In other applications, it is used as modifier for ABS crash pads and also as binder for brake linings.

CAS No: 9003-18-3

Information provided by LG Chemical

Vendors:
Available Properties
  • Specific Gravity
  • Volatiles
  • Mooney Viscosity, ML 1+4
  • Hardness, Shore A, Forming
  • Hardness, Shore A, Fuel Resistance
  • Hardness, Shore A, Heat Resistance
  • Hardness, Shore A, Fluid Aging ASTM Fuel D
  • Hardness, Shore A, Circulating Oven Aging
  • Tensile Strength at Break, Fuel Resistance
  • Tensile Strength at Break, Heat Resistance
  • Tensile Strength at Break, Forming
  • Tensile Strength at Break, Fluid Aging ASTM Fuel D
  • Tensile Strength at Break, Circulating Oven Aging
  • Elongation at Break, Forming
  • Elongation at Break, Heat Resistance
  • Elongation at Break, Fuel Resistance
  • Elongation at Break, Fluid Aging, ASTM Fuel D
  • Elongation at Break, Circulating Oven Aging
  • 300% Modulus, Forming
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.